GB/T12770 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures

Categories Stainless Steel Tube
Brand Name: TORICH
Model Number: GB/T12770
Certification: ISO9001:2008,ISO14001:2008
Place of Origin: China
MOQ: 5 ton
Price: negotiable
Payment Terms: L/C, D/A, D/P, T/T, Western Union, MoneyGram
Supply Ability: 50000Ton per year
Delivery Time: 30-35 work days
Packaging Details: in seaworthy packing
Material: Stainless Steel 201/304/316
Grade: S30210 S30408 S30403 S31008
Surface: pickling
Technique: Cold Rolled Cold Drawn
OD: 3-500mm
WT: 0.5-50mm
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

GB/T12770 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures

Product Name: GB/T12770 Material 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures


Size range: O.D.:3-500mm W.T.:0.5-50mm L:2000-12000mm according to customers' actual application and production.


Application : For Mechanical Structures purposes


Steel Grade: 12Cr18Ni9,06Cr19Ni10,022Cr19Ni10,06Cr25Ni20,022Cr22Ni5Mo3N,019Cr19Mo2NbTi,06Cr13Al


Characteristic:

Good concentricity

Good surface quality

Good OD and ID tolerance

High Precision

Stable quality

Smooth Roughness

TORICH QUALITY ASSURANCE


Table1Tolerance of OD

ClassificationNominal ODPermissible Tolerance
PCPBPA

H

T

<25±0.20±0.15±0.10
≥25~<40±0.30±0.25±0.20
≥40~<63±0.50±0.30±0.25
≥63~<90±0.60±0.50±0.40
≥90~<159±0.80±0.65±0.50
≥159~<300±0.8%D±0.7%D±0.5%D
≥300~<610±0.1%D±0.8%D±0.6%D
≥10protocolprotocolprotocol

WC

SP

<25±0.15±0.12±0.10
≥25~<40±0.20±0.15±0.13
≥40~<50±0.20±0.18±0.15
≥50~<60±0.25±0.20±0.18
≥60~<90±0.30±0.28±0.25
≥90~<100±0.40±0.35±0.30
≥100~<200±0.5%D±0.4%Dprotocol
≥200protocolprotocolprotocol

Table 2Tolerance of WT

Nominal WTPermissible Tolerance
<0.5±0..10
≥0.5~1.0±0.15
>1.0~2.0±0.20
>2.0~<4.0±0.30
≥4.0±10%S

Table 3 Bending Degree

Nominal Wall Thickness/mmBending Degree/(mm/m)
≤108≤1.0
>108~325≤1.5
>325≤2.5

Table4 The density of the steel and Calculation of Theoretic Weight

No.Steel GradeDensity/(kg/dm3)The formula after conversion
112Cr18Ni97.93W=0.02491S(D-S)
206Cr19Ni10
3022Cr19Ni107.90W=0.02482S(D-S)
406Cr25Ni207.98W=0.02507S(D-S)
506Cr17Ni12Mo28.00W=0.02513S(D-S)
6022Cr17Ni12Mo2
706Cr18Ni11Ti8.03W=0.02523S(D-S)
806Cr18Ni11Nb
9022Cr22Ni5Mo3N7.80W=0.02450S(D-S)
10022Cr23Ni5Mo3N
11022Cr25Ni7Mo4N
12022Cr18Ti7.70W=0.02491S(D-S)
13019Cr19Mo2NbTi7.75W=0.02435S(D-S)
1406Cr13Al
15022Cr11Ti
16022Cr12Ni
1706Cr13

Table 5 Steel Grade and Chemical Componenet

No.TypeUnified digital codeGradeChemical Componenet(Quality Fraction)/%
CSiMnPSNiCrMoNOthers
1AusteniteS3021012Cr18Ni9≤0.15≤0.75≤2.00≤0.040≤0.0308~1017~19-≤0.10-
2S3040806Cr19Ni10≤0.08≤0.75≤2.00≤0.040≤0.0308~1118~20---
3S30403022Cr19Ni10≤0.030≤0.75≤2.00≤0.040≤0.0308~1218~20---
4S3100806Cr25Ni20≤0.08≤1.50≤2.00≤0.040≤0.03019~2224~26---
5S3160806Cr17Ni12Mo2≤0.08≤0.75≤2.00≤0.040≤0.03010~1416~182~3--
6S31603022Cr17Ni12Mo2≤0.08≤0.75≤2.00≤0.040≤0.03010~1416~182~3--
7S3216806Cr18Ni11Ti≤0.08≤0.75≤2.00≤0.040≤0.0309~1217~19--Ti15C~0.70
8S3477806Cr18Ni11Nb≤0.08≤0.75≤2.00≤0.040≤0.0309~1217~19--Nb110C~1010
9BipolarS22253022Cr22Ni5Mo3N≤0.030≤1.00≤2.00≤0.030≤0.0204.5~6.521~232.5~3.50.08~0.20
10S22053022Cr23Ni5Mo3N≤0.030≤1.00≤2.00≤0.030≤0.0204.5~6.522~233~3.50.14~0.20
11S25073022Cr25Ni7Mo4N≤0.030≤0.80≤1.20≤0.035≤0.0206~824~263~50.24~0.32Cu≤0.50
12FerriteS11863022Cr18Ti≤0.03≤0.75≤1≤0.04≤0.03(0.60)16~19--Ti or Nb:0.1~1
13S11972019Cr19Mo2NbTi≤0.025≤0.75≤1≤0.04≤0.031.0017.5~19.501.75~2.50≤0.035(Ti+Nb):[0.2+4(C+N)]~0.8
14S1134806Cr13Al≤0.08≤0.75≤1≤0.04≤0.03(0.60)11.50~14.50--Al:0.1~0.3
15S11163022Cr11Ti≤0.03≤0.75≤1≤0.04≤0.02(0.60)10.50~11.70-≤0.030Ti≥8(C+N),Ti:0.15~0.50,Nb≤0.10
16S11213022Cr12Ni≤0.03≤0.75≤1.5≤0.04≤0.0150.3~1.0010.50~12.50-≤0.030
17MartensiticS4100806Cr13≤0.08≤0.75≤1≤0.04≤0.03(0.60)11.50~13.50---
Note:The number in brackets is the maximum allowed to be added. Chemical component of some grade is different from GB/T20878.

Table 6 Recommendatory heat treating regime of the steel tubes

No.TypeSteel gradeRecommendatory heat treating regime
1Austenite12Cr18Ni91010℃~1150℃,water-cooling or other methods of rapid cooling
206Cr19Ni101010℃~1150℃,water-cooling or other methods of rapid cooling
3022Cr19Ni101010℃~1150℃,water-cooling or other methods of rapid cooling
406Cr25Ni201030℃~1180℃,water-cooling or other methods of rapid cooling
506Cr17Ni12Mo21010℃~1150℃,water-cooling or other methods of rapid cooling
6022Cr17Ni12Mo21010℃~1150℃,water-cooling or other methods of rapid cooling
706Cr18Ni11Ti920℃~1150℃,water-cooling or other methods of rapid cooling
806Cr18Ni11Nb980℃~1150℃,water-cooling or other methods of rapid cooling
9Dual-phase steel022Cr22Ni5Mo3N1020℃~1100℃,water-cooling
10022Cr23Ni5Mo3N1020℃~1100℃,water-cooling
11022Cr25Ni7Mo4N1025℃~1125℃,water-cooling
12Ferritic022Cr18Ti780℃~950℃,rapid cooling or slow cooling
13019Cr19Mo2NbTi800℃~1050℃,rapid cooling
1406Cr13Al780℃~830℃,rapid cooling or slow cooling
15022Cr11Ti800℃~900℃,rapid cooling or slow cooling
16022Cr12Ni700℃~820℃,rapid cooling or slow cooling
17Martensite06Cr13750℃,rapid cooling ;800℃~900℃,slow cooling

Buy GB/T12770 12Cr18Ni9 019Cr19Mo2NbTi Welded Stainless Steel Tubes for Mechanical Structures at wholesale prices
Send your message to this supplier
 
*From:
*To: TORICH INTERNATIONAL LIMITED
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0