| Sign In | Join Free | My benadorassociates.com |
|
| Categories | Metal Wire Mesh |
|---|---|
| Brand Name: | Ohmalloy |
| Model Number: | 1J79 |
| Certification: | ISO,SGS |
| Place of Origin: | SHANGHAI |
| MOQ: | 20kg |
| Price: | usd 10-20/kg |
| Payment Terms: | L/C, D/A, D/P, T/T, , MoneyGram |
| Supply Ability: | 5000kg/month |
| Delivery Time: | 7-20days |
| Packaging Details: | in wooden box |
| material: | 1J79 |
| brand: | Ohmalloy |
| color: | Primary Color |
| wire diameter: | 0.02mm-0.8mm |
| delivery time: | 7-20days |
| package: | wooden box |
| sample: | free sample |
| alloy or not: | is alloy |
| Company Info. |
| Ohmalloy Material Co.,Ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
1J79 soft magnetic wire mesh,OEM types of weave,for shielding
Normal composition
| Ni | 78.5~80.0 | Fe | Bal. | Mn | 0.6~1.1 | Si | 0.3~0.5 |
| Mo | 3.8~4.1 | Cu | ≤0.2 | ||||
| C | ≤0.03 | P | ≤0.02 | S | ≤0.02 |
| Yield strength | Tensile Strength | Elongation |
| Mpa | Mpa | % |
| 980 | 1030 | 3~50 |
| Density (g/cm3) | 8.6 |
| Electrical resistivity at 20℃(Ωmm2/m) | 0.55 |
| Coefficient of linear expansion(20℃~200℃)X10-6/℃ | 10.3~11.5 |
| Saturation magnetostriction coefficient λθ/ 10-6 | 2.0 |
| Curie point Tc/ ℃ | 450 |
The magnetic properties of alloys with high permeability in weak fields | |||||||
| 1J79 | Initial permeability | Maximum permeability | Coercivity | Saturation magnetic induction intensity | |||
Сold-rolled strip/ sheet. Thickness, mm | μ0.08/ (mH/m) | μm/ (mH/m) | Hc/ (A/m) | BS/ T | |||
| ≥ | ≤ | ||||||
| 0.01 mm | 17.5 | 87.5 | 5.6 | 0.75 | |||
| 0.1~0.19 mm | 25.0 | 162.5 | 2.4 | ||||
| 0.2~0.34 mm | 28.0 | 225.0 | 1.6 | ||||
| 0.35~1.0 mm | 30.0 | 250.0 | 1.6 | ||||
| 1.1~2.5 mm | 27.5 | 225.0 | 1.6 | ||||
| 2.6~3.0 mm | 26.3 | 187.5 | 2.0 | ||||
| cold drawn wire | |||||||
| 0.1 mm | 6.3 | 50 | 6.4 | ||||
| Bar | |||||||
| 8-100 mm | 25 | 100 | 3.2 | ||||