2205 S32205 Stainless Steel Bar Round / Square / Hexagon Shape Stress Corrosion Resistant

Categories Stainless Steel Bar
Brand Name: BOZHONG
Model Number: 2205/S32205
Certification: ISO/TUV/DNV
Place of Origin: CHINA
MOQ: negotiable
Price: negotiable
Payment Terms: L/C, T/T, Western Union, MoneyGram
Supply Ability: 10000TON/MONTH
Delivery Time: 3--10days
Packaging Details: seaworthy packing
GRADE: S32205
SURFACE: BLACK/BRIGHT
LENGTH: 6000/5000--7000mm
SHAPE: round/squre/hexagon/bar/rod
Description: stainless steel bar
Material: duplex stainless steel
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

2205 S32205 Stainless Steel Bar Round / Square / Hexagon Shape Stress Corrosion Resistant

Stainless steel bar

Equivalent designations
UNS S32205
DIN W. Nr. 1.4462


FormASTM
Rod, bar and shapeA 276, A 484
Plate, sheet and stripA 240, A 480
Seamless and welded pipeA 790, A 999
Seamless and welded tubingA 789, A 1016
FittingA 815, A 960
Forged or rolled pipe flange and forged fittingA 182, A 961
Billet and bar for forgingA 314, A 484
Chemical composition
%FeCrNiMoCMnSiPSN
minbalance224.530.14
max236.53.50.03210.030.020.2
Physical properties
Density7.69 g/cm3
Melting range1385-1443℃

Features:

2205 is a duplex stainless steel with nearly equal proportions of austenite and ferrite when properly heat treated. This microstructure makes it much more resistant to stress corrosion cracking than stainless steel 304 and 316L. 2205’s higher chromium, molybdenum and nitrogen contents give it significantly improved pitting and crevice corrosion resistance in the presence of chlorides. Its yield strength is about twice that of austenitic stainless steels. It is highly suitable for Applications in environments containing chlorides and hydrogen sulfide such as marine applications and oil and gas production.


Applications:

Oil and gas industry piping, tubing and heat exchangers; pulp and paper industry bleaching equipment, liquor tanks and digesters; cargo tanks for ships and trucks; chemical processing industry pressure vessels, tanks, piping and heat exchangers; and food processing equipment.


Product Tags:

ss bar stock

  

stainless steel rod

  
Buy 2205 S32205 Stainless Steel Bar Round / Square / Hexagon Shape Stress Corrosion Resistant at wholesale prices
Send your message to this supplier
 
*From:
*To: Shanghai Bozhong Metal Group Co., Ltd.
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0