| Sign In | Join Free | My benadorassociates.com |
|
| Categories | FeCrAl Alloy |
|---|---|
| Brand Name: | OHMALLOY/OEM |
| Model Number: | SP-235-spring |
| Certification: | ISO9001:2015 |
| Place of Origin: | China |
| MOQ: | 50KG |
| Payment Terms: | L/C, T/T, , PayPal |
| Supply Ability: | 30000 KG per Month |
| Delivery Time: | 5-18 working days after payment confirmed |
| Packaging Details: | plywood pallet or plywood case |
| Name: | FeCrAl135 Heating Spring Wire 0Cr23Al5 Long Service Life Good Processing Performance |
| Supply State: | Wire or Spring(as customer requirements) |
| Application: | Home Appliance Heating Spring Wire |
| Resistance: | As customer requirements |
| MOQ: | 20KG(Wire) 500pieces(spring) |
| Warranty: | 2 years |
| Package: | Plywood Case |
| Company Info. |
| Ohmalloy Material Co.,Ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
FeCrAl135 Heating Spring Wire 0Cr23Al5 Long Service Life Good Processing Performance
Common Name:0Cr23Al5, D, , Alloy 815, Alchrome DK, Alferon 901,
Resistohm 135,Aluchrom S, Stablohm 812)
OhmAlloy135 is a iron-chromium-aluminium alloy (FeCrAl alloy)
characterized by high resistance, low coefficient of electric
resistance, high operating temperature, good corrosion resistance
under high temperature.It is suitable for use at temperatures up to
1250°C.
Typical applications for OhmAlloy135 are used in home appliances
and industrial furnace,and kinds of elements in heaters and dryers.
| C | P | S | Mn | Si | Cr | Ni | Al | Fe | Other |
| Max | |||||||||
| 0.06 | 0.025 | 0.025 | 0.70 | Max 0.6 | 20.5~23.5 | Max 0.60 | 4.2~5.3 | Bal. | - |
| Yield strength | Tensile Strength | Elongation |
| Mpa | Mpa | % |
| 485 | 670 | 23 |

Typical Physical properties
| Density (g/cm3) | 7.25 |
| Electrical resistivity at 20℃(Ωmm2/m) | 1.35 |
| Conductivity coefficient at 20℃ (WmK) | 13 |
| Coefficient of thermal expansion | |
| Temperature | Coefficient of Thermal Expansion x10-6/℃ |
| 20 ℃- 1000℃ | 15 |
| Specific heat capacity | |
| Temperature | 20℃ |
| J/gK | 0.46 |
| Melting point (℃) | 1500 |
| Max continuous operating temperature in air (℃) | 1250 |
| Magnetic properties | non-magnetic |
|