| Sign In | Join Free | My benadorassociates.com |
|
| Categories | Precision Alloy |
|---|---|
| Brand Name: | Tankii |
| Model Number: | Alloy 52 |
| Certification: | ISO9001:2015 |
| Place of Origin: | Shanghai, China |
| MOQ: | 20kg |
| Price: | Negotiated price |
| Payment Terms: | L/C, T/T, Western Union, MoneyGram, Paypal |
| Supply Ability: | 200+TON+MONTH |
| Delivery Time: | 7-12 DAYS |
| Packaging Details: | Spool in carton, if necessary with plywood pallet o plywood case or according to client´s requirements |
| Material: | Ferronickel |
| Treatment: | Annealed, cold drawing |
| Nickel: | 50.5% |
| Use: | Glass-Metal Sealing |
| Resistance: | Uniform |
| Color: | Bright |
| Company Info. |
| Shanghai Tankii Alloy Material Co.,Ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
Alloy 52 0.25mm*0.64mm Precision Alloy Flat Wire/ Ribbon Wire
General Information:
Applications for Alloy 52 include magnetic reed switches and seals
that need controlled linear expansion to approximately 977 °F (525
°C).
Alloy 52 is a 50.50% nickel-iron alloy developed for glass-to-metal
seals for some of the soft glasses and some ceramics. The alloy's
rate of thermal expansion is virtually constant to a temperature of
about 1050 °F (565 °C).
Carbon: 0.05 max
Silicon: 0.30 max
Manganese: 0.60 max
Nickel: 50.5 nom
Chromium: 0.25 max
Iron: Balance
Phosphorus: 0.025 max
Sulfur: 0.025 max
Aluminum: 0.10 max
| Chemical compositions(%) | ||
| Alloy | Ni | Fe |
| 4J42 | 41.5~42.5 | rest |
| 4J45 | 44.5~45.5 | rest |
| 4J50 | 49.5~50.5 | rest |
| 4J52 | 51.5~52.5 | rest |
| 4J54 | 53.5~54.5 | rest |
Density: 0.30 lb/in3, 8.30 g/cm3
Electrical Resistivity: ohm-cir-mil/ft, microhm-cm:
At 68 °F (20 °C): 258 (43)
Thermal Conductivity: BTU-in/hr-ft2-°F (W/m•K):
68 - 212 °F (20 - 100 °C): 97 (140)
Mean Coefficient of Thermal Expansion: µin/in-°F (µm/m-°C):
77 - 842 °F (25 - 450 °C): 5.4 (9.8)
Melting Range: 2600 °F (1430 °C)
Coil - Sheet, Strip, Ribbon
Wire - Profile, Round, Flat, Square
Ultimate Tensile Strength: 78 KSI nom (536 MPa nom)
Yield Strength: 35 KSI nom (240 MPa nom)
Elongation: 30% nom
Hardness: Rb 73 nom
Alloy 52 can be cold worked to various tempers. Contact Ulbrich Technical Service for additional information.
Refer to NACE (National Associate of Corrosion Engineers) for recommendations.
#1 - Hot rolled annealed and descaled. It is available in strip,
foil and ribbon. It is used for applications where a smooth
decorative finish is not required.
#2D - Dull finish produced by cold rolling, annealing and
descaling. Used for deep drawn parts and those parts that need to
retain lubricants in the forming process.
#2B - Smooth finish produced by cold rolling, annealing and
descaling. A light cold rolling pass is added after anneal with
polished rolls giving it a brighter finish than 2D.
#BA - Bright annealed cold rolled and bright annealed
#CBA - Course bright annealed cold rolled matte finish and bright
anneal
#2 - Cold Rolled
#2BA- Smooth finish produced by cold rolling and bright annealing.
A light pass using highly polished rolls produces a glossy finish.
A 2BA finish may be used for lightly formed applications where a
glossy finish is desired in the formed part.
Polished - Various grit finish for specific polish finished
requirements.




|