| Brand Name: | MEILONG |
| Model Number: | 1/4'' OD x 0.065'' WT |
| Certification: | ISO9001:2015, PED 97/23/EC |
| Place of Origin: | China |
| MOQ: | 10000 feet |
| Payment Terms: | L/C, T/T |
| Supply Ability: | 150000 meters per month |
| Delivery Time: | 10 days (for our required MOQ) |
| Packaging Details: | Level wound coiled on wooden spool, and wooden case packing |
| Material: | TP316L comply with NACE MR0175/ISO15156 |
| Tube type: | Seamless |
| Condition: | Bright annealed |
| Length: | Up to 10000 meters long per reel |
| Qualification: | Hydrostatic tested |
| Application: | Oil and gas fields |
| Surface: | Metallic bright |
| Specialty: | High-pressure hydraulic |
| Price: | Negotiable |
| Company Info. |
| Suzhou Vanforge Metals Co., Ltd. |
| View Contact Details |
| Product List |
Stainless Steel TP316L Seamless Precision Coil Tubing Bright Annealed Stress Corrosion
TP316L, Chemical composition
| Element | Composition, % |
| Chromium | 16.0-18.0 |
| Nickel | 10.0-14.0 |
| Molybdenum | 2.0-3.0 |
| Manganese | 2.00 max. |
| Silicon | 1.00 max. |
| Carbon | 0.035 max. |
| Sulfur | 0.030 max. |
| Phosphorous | 0.045 max. |
Application: Standard oil and gas CRA (corrosion resistant alloy)
Tensile strength, min.: 70ksi (485MPa)
Yield strength, min.: 25ksi (170MPa)
Elongation in 2 in., min.: 35%
Application (seamless tubing)
TP316L seamless pressure tubing in the heat treated condition is typically used in oil and natural gas wells for applications including hydraulically-actuated surface-controlled subsurface safety valves, chemical injection, and instrumentation. In such applications, it is commonly referred to as control line tubing. The tubing is generally deployed by strapping it to the outside of the production casing. It may be encapsulated and can be included along with other pressure or TEC and mechanical components, such as bumpers, within a flatpack. The tubing is frequently supplied as 5,000 to 35,000 ft. coils on a wooden or steel reel, depending on size.
HYDRAULIC AND INSTRUMENTATION APPLICATIONS
STAINLESS STEEL AND HIGH NICKEL ALLOYS COILED TUBING SOLUTIONS
MEILONG is an important manufacturer in premium coiled seamless & welded tubular solutions for oil and gas applications. In an endeavor to increase its presence in subsea, MEILONG has extended its offer by developing a highly innovative tubular solution for umbilical projects.
MEILONG has developed a strong and unique expertise in premium quality tubes to answer the most stringent specifications of its customers. Based on this expertise in high pressure, and extremely high pressure tubes, MEILONG’s state-of-art factory is exclusively dedicated to the manufacturing and supply of super duplex and high nickel alloys tubes for corrosive downhole applications and is now ready to offer the highest specifications for your toughest challenges.
NDT
Full online and real time controls
100% of tube length & circumference Eddy Current & Ultrasonic Testing
Inhouse Laboratory
Mechanical testing
Metallurgical testing
Dimensional controls
MEILONG has been supplying the world’s best coiled tubes up to 3,234 lbs (1,467 kgs) and 14,764 ft (4500 mtrs) length without orbital butt welding.
Bright annealing treated, our coiled tubes are excellent in both internal and external surface quality.
Our coiled tubes are specially used in oil and gas industry requiring a higher level of reliability.
All the products are performed and delivered after ECT as well as hydrostatic & ovality test satisfying ASTM standards.
| Materials | Imperial Size | Metric Size | |||
OD (in.) | WT (in.) | OD (mm) | WT (mm) | ||
SS316L Duplex 2205 Super Duplex 2506 Incoloy 825 Inconel 625 | 1/8 | 0.125 | 0.028 | 3.18 | 0.71 |
| 1/8 | 0.125 | 0.035 | 3.18 | 0.89 | |
| 1/4 | 0.250 | 0.035 | 6.35 | 0.89 | |
| 1/4 | 0.250 | 0.049 | 6.35 | 1.24 | |
| 1/4 | 0.250 | 0.065 | 6.35 | 1.65 | |
| 3/8 | 0.375 | 0.035 | 9.53 | 0.89 | |
| 3/8 | 0.375 | 0.049 | 9.53 | 1.24 | |
| 3/8 | 0.375 | 0.065 | 9.53 | 1.65 | |
| 3/8 | 0.375 | 0.083 | 9.53 | 2.11 | |
| 1/2 | 0.500 | 0.049 | 12.70 | 1.24 | |
| 1/2 | 0.500 | 0.065 | 12.70 | 1.65 | |
| 1/2 | 0.500 | 0.083 | 12.70 | 2.11 | |
| 5/8 | 0.625 | 0.049 | 15.88 | 1.24 | |
| 5/8 | 0.265 | 0.065 | 15.88 | 1.65 | |
| 5/8 | 0.625 | 0.083 | 15.88 | 2.11 | |
| 3/4 | 0.750 | 0.049 | 19.05 | 1.24 | |
| 3/4 | 0.750 | 0.065 | 19.05 | 1.65 | |
| 3/4 | 0.750 | 0.083 | 19.05 | 2.11 | |
Applied Standard
ASTM A213: Standard specification for seamless and austenitic alloy-steel boiler, superheater, and heat exchanger tubes
ASTM A262: Practices for detecting susceptibility to intergranular attack in austenitic stainless steels
ASTM A269: Standard specification for seamless and welded, austenitic stainless steel tubing for general use
ASTM A370: Test methods and definitions for mechanical testing of steel products
ASTM A450: Standard specification for general requirements for carbon, ferritic alloy, and austenitic alloy steel tubes
ASTM A632: Standard specification for seamless and welded, austenitic stainless steel tubing (small diameter) for general use
NACE MR 0175: Selection and qualification of carbon and low-alloy steels, corrosion-resistant alloys, and other alloys for service in equipment in oil and natural gas production and NG treatment plants in H2S-containing environment
EN10204: Inspection documents for metallic products
Description
TP316L is a chromium - nickel austenitic stainless steel with an addition of molybdenum and reduced carbon content. The addition of molybdenum provides improved resistance to pitting and crevice corrosion in environments containing halides such as chlorides when compared to so-called conventional 18 chromium 8 nickel austenitic stainless steels such as 304L. The reduced carbon content minimizes harmful chromium carbide precipitation during welding and thereby improves resistance to intergranular corrosion. Austenitic stainless steels such as 316L are susceptible to stress corrosion cracking (SCC) in environments containing chlorides and other halides. Alloy 316L is generally used in oil and gas production environments which do not contain oxygen and have limited amounts of chlorides and hydrogen sulfide. Consult ISO 15156-3, Table A.2 for the limits regarding alloy 316L in hydrogen sulfide containing environments for oil and gas production.
Manufacturing Process and Resultant Properties
Seamless extruded tube hollows are drawn or drawn / sunk to final size to produce seamless tubing coils 500 to 2,000 ft. long, depending upon the size. The tubing is heat treated and joined by orbital welding to achieve the desired length. The final material condition of the tubing is heat treated.
Nondestructive Testing (NDT)
Eddy current testing (ECT) is performed at final size in the heat treated condition. Radiographic testing is performed on all orbital welds. Yield pressure hydrostatic testing is performed on the heat treated tubing at final size.
Quality Assurance
Eddy current test (ECT)
Ultrasonic test
Hydrostatic test
Chemical composition analysis
Tensile test
Hardness test
Dimension & visual inspect
Metallographic analysis
Standards and Specifications
ASTM A269, Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service
Meets the material limits for 316L austenitic stainless steel listed in ISO 15156-3, Table A.2.
Norm Equivalence
| Grade | UNS No | Euro norm | Japanese | |
| No | Name | JIS | ||
| Alloy | ASTM/ASME | EN10216-5 | EN10216-5 | JIS G3463 |
| 316L | S31603 | 1.4404, 1.4435 | X2CrNiMo17-12-2 | SUS316LTB |
| 2205 | S31803 | 1.4462 | X2CrNiMoN22-5-3 | SUS329J3LTB |
| 2507 | S32750 | 1.4410 | X2CrNiMoN25-7-4 | |
| 625 | N06625 | 2.4856 | NiCr22Mo9Nb | |
| 825 | N08825 | 2.4858 | NiCr21Mo | |




|