Sign In | Join Free | My benadorassociates.com
benadorassociates.com
Products
Search by Category
Home > Nickel >

Anti Oxidation INCOLOY Alloy 825 Alloy Round Bar 825 Tubing Superalloy

Categories Alloy Round Bar
Brand Name: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number: INCOLOY alloy 825
Certification: SGS,TUV,BV,ISO,MTC
Place of Origin: China
MOQ: Negotiations
Price: Negotiations
Payment Terms: T/T
Supply Ability: 100000KGS/Month
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 45-55days
Packaging Details: Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Product Name: INCOLOY alloy 825 Alloy Round Bar
Grades: INCOLOY alloy 825
Processing methods: Shot blasted,Cold working,Machined,etc
Surface: Black,Grinding,Centreless Ground,etc
Profile: Round Bar,Sheets Plates,Forging Piece,etc
Price Term: Ex-work,FOB,DDU etc.
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

Anti Oxidation INCOLOY Alloy 825 Alloy Round Bar 825 Tubing Superalloy

INCOLOY alloy 825 Alloy Round Bar 825 Superalloy Round Bar 825 Round Bar 825 Bar


Description


Our company provides INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar.

All of INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.


  • Material:Metal,INCOLOY alloy 27-7Mo Alloy Round Bar INCOLOY alloy 27-7Mo Round Bar 27-7Mo Bar
  • Shape:Superalloy Round Bar
  • Round bar / Wire rod (Diameter): 5.5mm to 800mm

  • Square bar / Flat bar: 3mm to 800mm

  • Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm

  • Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)


Products Details


INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar

Chemical Composition (weight%):Mechanical Properties Under Final Heat Treatment:

C (%): ≤ 0.04
Cr (%):≤ 21.0
Ni (%):≤42.0
Mo (%): ≤3.00
Cu (%):≤2.00

Ti(%):≤1.00

Fe(%):≤30.0

Condition: Solution annealed
Tensile strength, σb/≥ MPa: 586
Yield strength, σ0.2/≥ MPa: 241
Elonghation, δ ≥(%): 30.0


Applications:


INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar,Tall oil distillation columns and equipments,etc


INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar


FAQ


Q: How do you control the quality?


A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


Q: Do you accept customization?


A: Yes. If you have special requirements for products or packaging, we can make them for you.


Q: Can you accept trial orders?


A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


Q: How do I get samples?


A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.



Wooden Pallet BOX,based on the customer's special requirement,Standard Seaworthy Package,etc

Buy Anti Oxidation INCOLOY Alloy 825 Alloy Round Bar 825 Tubing Superalloy at wholesale prices
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0