| Sign In | Join Free | My benadorassociates.com |
|
| Categories | Grinding Cylpebs |
|---|---|
| Brand Name: | HUAFU |
| Model Number: | Dia.20MM-160MM |
| Certification: | GB/T 19001-2016/ISO 9001:2015 |
| Place of Origin: | China |
| MOQ: | 1 Ton |
| Price: | $ 790/Mt |
| Payment Terms: | L/C, T/T, D/P, D/A |
| Supply Ability: | The annual output is 150,000 tons |
| Delivery Time: | 2-4 weeks |
| Packaging Details: | Bag or iron drum |
| Diameter: | 20×25mm-50×55mm |
| Impact value: | ≥5-7J/cm² |
| Hardness: | 45-58HRC |
| Breakage rate: | ≤1% |
| Drop times: | ≥12000 |
| Micri structure: | M+C |
| Company Info. |
| Jinan Huafu Forging Joint-Stock Co.,ltd. |
| Verified Supplier |
| View Contact Details |
| Product List |
Fine Grinding Hot Rolling Grinding Cylpebs Casting Grinding Cylpebs For Ball Mill

COMPANY ENVIOMENT

PRODUCTS INTRODUCTION
High Chrome casting steel ball
High chrome casting grinding ball, chrome concentration is 10%-24%, hardness ≥HRC58. High chrome casting grinding ball is one of the wearable steel ball with better performance-price-ratio, and its extensive usage has won itself a high share in the market.
Chemical Composition | C(%) | Si(%) | Mn(%) | Cr(%) | Cu(%) | Mo(%) | P(%) | S(%) |
| 2.0-3.3 | ≤1.2 | 0.3-1.5 | 10.0-24.0 | ≤1.2 | ≤3.0 | ≤0.10 | ≤0.10 |
Medium chrome casting steel ball
Middle chrome grinding balls chrome concentration is 4-6%, hardness ≥ HRC 48, Middle chrome grinding ball have a better performance than complex alloy ball.
Chemical Composition | C(%) | Si(%) | Mn(%) | Cr(%) | Cu(%) | Mo(%) | P(%) | S(%) |
| 2.1-3.6 | ≤1.5 | 0.3-1.5 | 4.0-6.0 | ≤0.80 | ≤1.0 | ≤0.10 | ≤0.10 |
Low chrome casting steel ball
Chrome Concentration is 1-3%, hardness ≥ HRC 45, this steel ball is called low chrome grinding balls, which is made by smelting in intermediate frequency electric furnace, metal mould or sand casting process. It applies to metallurgic mines and slag industries where no high grinding accuracy or wearability is required.
Chemical Composition | C(%) | Si(%) | Mn(%) | Cr(%) | Cu(%) | Mo(%) | P(%) | S(%) |
| 2.1-3.6 | ≤1.5 | 0.3-1.5 | 1.0-3.0 | ≤0.80 | ≤1.0 | ≤0.10 | ≤0.10 |
Production process of grinding rod
Raw material inspection →Blanking→Burr grinding→intermediate frequency furnace heating→straightening→Quenching treatment→Tempering treatment→Finished products inspection→packing