| Boiling Point: | 4639°C |
| Density: | 10.2 g/cm3 |
| Electrical Conductivity: | 35% IACS |
| Electrical Resistivity: | 6.99μΩ.m |
| Molybdenum Melting Poin: | 2620 °C |
| Stanadrd: | ASTM B387 |
| Tensile Strength: | 585 MPa |
| Thermal Conductivity: | 138 W/m·K |
| Company Info. |
| Luoyang Hypersolid Metal Tech Co., Ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
1,Description:
Molybdenum bars are solid cylindrical rods made from molybdenum, a refractory metal known for its high melting point and excellent mechanical properties. These bars are widely used in various industries, including aerospace, electronics, and power generation, due to their unique combination of strength, high-temperature resistance, and conductivity.
Molybdenum bars exhibit exceptional strength and hardness, making them suitable for applications that require materials capable of withstanding high mechanical stress and deformation. They have a high melting point of 2,617°C (4,723°F), which allows them to maintain their structural integrity and performance at elevated temperatures.
2,Specifications:
| Density | 10.2 g/cm³ (at 20°C) |
| Melting Point | 2,617°C (4,723°F) |
| Thermal Conductivity | 138 W/m·K (at 20°C) |
| Coefficient of Thermal Expansion | 4.8 x 10^-6 /°C (at 20-1,000°C) |
| Electrical Conductivity | 35% IACS (International Annealed Copper Standard) (at 20°C) |
| Hardness (Rockwell C) | 30 - 40 HRC |
| Tensile Strength | 585 - 760 MPa |
| Yield Strength | 415 - 620 MPa |

|