ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking

Categories Others
Brand Name: YUHONG
Model Number: ASTM A240 904L
Certification: ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008
Place of Origin: CHINA
MOQ: 1pcs
Price: Negotiable
Payment Terms: L/C, T/T
Supply Ability: 1000Tons/Month
Delivery Time: 7DAYS
Packaging Details: Ply-wooden Case /Iron Case/ Bundle with plastic Cap
Product Name: Stainless Steel Plate, Sheet
Standard: ANSI, ASTM, ASME, JIS, DIN, EN
Material: Stainless Steel 904L
Width: As Resquest
Finish: Polished, Mirror, Bright, Hairline, Satin, Brushed, Ect.
Packing: Water Proof And Seaworthy Package
Company Info.
Yuhong Group Co.,Ltd
Verified Supplier
View Contact Details
Product List
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking

ASTM A240 904L NO8904 Stainless Steel Plate Sheet Coil


ASTM A240 is a specification for stainless steel plate, sheet, and strip for pressure vessels and for general applications. It covers grades such as 304, 304L, 316, 316L, 321, 347, and 904L.

Stainless steel 904L is a low carbon, high alloy austenitic stainless steel with excellent corrosion resistance. It is commonly used in chemical processing, oil and gas production, and other demanding environments where corrosion resistance is critical.

ASTM A240 stainless steel 904L plate is available in various thicknesses, widths, and lengths. It is typically supplied in the annealed condition and can be further heat treated to enhance its properties.

The mechanical properties of ASTM A240 stainless steel 904L plate include a tensile strength of 490 MPa (71 ksi), a yield strength of 220 MPa (32 ksi), and an elongation of 35%.


The execution standard for 904L seamless steel pipe is ASTM A240/ASME
904L belongs to austenitic stainless steel, with physical and mechanical properties: density: 8.24g/cm3. Tensile strength: σ B ≥ 520Mpa. Elongation: δ≥ 35%.It has good resistance to spot corrosion and Crevice corrosion, high resistance to stress corrosion cracking, good resistance to intergranular corrosion, good workability and weldability.


904L is a low-carbon austenitic stainless steel that can be used under severe corrosion conditions. It contains 25% nickel and 4.5% molybdenum, and has good resistance to chloride stress corrosion cracking. Compared with 316L and 317L, 904L has excellent corrosion resistance. Due to the addition of Cu, the alloy exhibits excellent corrosion resistance to reducing acids such as sulfuric acid and phosphoric acid.
Common applications include the production and transportation of sulfuric acid, metal pickling in sulfuric acid, papermaking and related industries, and the chemical and pharmaceutical industries.


ASTM A240 SS904L Stainless Steel Plate Chemical Composition


ElementSS 904L
C0.020 max
Mn2 max
Si1 max
P0.040 max
S0.030 max
Cr19 – 23
Ni23 – 28
Mo4 – 5
Cu1 – 2

ASTM A240 SS904L Stainless Steel Plate Mechanical Properties


ElementSS 904L
Density7.95 g/cm3
Melting Point1350 °C (2460 °F)
Tensile StrengthPsi – 71000 , MPa – 490
Yield Strength (0.2%Offset)Psi – 32000 , MPa – 220
Elongation35%

Material Testing


1. Chemical processing

2. Oil and gas industry

3. Desalination plants

4. Food processing industry

5. Marine industry

6. Heat exchangers

7. Petrochemical industry



Buy ASTM A240 Stainless Steel 904L Plate With High Resistance To Stress Corrosion Cracking at wholesale prices
Send your message to this supplier
 
*From:
*To: Yuhong Group Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0