| Sign In | Join Free | My benadorassociates.com |
|
| Categories | Stainless Steel Seamless Tube |
|---|---|
| Brand Name: | TSING SHAN |
| Model Number: | Sanicro 28 |
| Certification: | ISO SGS MTC |
| Place of Origin: | China |
| MOQ: | 100KGS |
| Price: | 31.5 USD/KG |
| Payment Terms: | L/C, T/T |
| Supply Ability: | 50000KGS |
| Delivery Time: | 7 Days |
| Packaging Details: | Export Packing |
| Package: | Wooden Box, Steel Pallet, etc. |
| Third Party Inspection: | BV,SGS,ASP |
| Item: | Sanicro 28 Stainless Steel Tube |
| Payment Term: | 30%TT+70%TT / LC |
| Applications: | Construction,Industry,boiler,Chemical |
| Condition: | Soft / Hard |
| Appllication: | heat exchanger/ chemical |
| Company Type: | factory and trading |
| Ends: | Plain End, Beveled End, Threaded End |
| Test: | 100% NDT |
| Packing: | Standard Sea-worthy Packing |
| Products: | stainless steel pipe |
| Application: | Industrial, Automotive, Construction |
| Secondary Or Not: | Non-secondary |
| Color: | natural color |
| Company Info. |
| TSING SHAN STEEL INDUSTRIAL LIMITED |
| Verified Supplier |
| View Contact Details |
| Product List |
Alloy 28 (UNS N08028, W. Nr. 1.4563, Sanicro 28) is a
nickel-iron-chromium alloy with additions of molybdenum and copper.
It has excellent resistance to both reducing and oxidizing acids,
to stress-corrosion cracking, and to localise attack such as
pitting and crevice corrosion. The alloy is especially resistant to
sulphuric and phosphoric acid. Used for chemical processing,
pollution control equipment, oil and gas well piping, nuclear fuel
reprocessing, acid production and pickling equipment.
▪ Chemical and petrochemical processing industry
▪ Downhole service in deep sour gas wells.
Incoloy 28 Chemical Composition
| Element | Content (%) |
| Iron, Fe | 29-40.4 |
| Nickel, Ni | 30-34 |
| Chromium, Cr | 26-28 |
| Molybdenum, Mo | 3-4 |
| Manganese, Mn | ≤2.5 |
| Others | Remainder |
| Properties | Metric | Imperial |
| Tensile strength(annealed) | 500 MPa | 72.5 ksi |
| Yield strength(annealed) | 214 MPa | 31 ksi |
| Elongation at Break(Cold worked) | 15% | 50% |
| Modulus of Elasticity | 200 GPa | 29000 ksi |
| Hardness, Rockwell B | 80-90 | 80-90 |
| Hardness, Rockwell C | 33 | 33 |
| Incoloy 28 available sizes and specifications | |
| Grade | Incoloy 28 |
| Nickel plate | Thickness: 0.3mm - 150.0mm Width: 1000mm - 3000mm |
| Nickel strip/ nickel foil | Thickness: 0.02mm - 16.0mm Width: 5mm - 3000mm |
| Nickel coil | Thickness: 0.3mm - 16.0mm Width: 1000mm - 3000mm |
| Nickel pipe | Outside diameter: 6mm - 1219mm Thickness: 0.5mm - 100mm |
| Nickel Capillary Pipe | Outside diameter: 0.5mm - 6.0mm Thickness: 0.05mm - 2.0mm |
| Nickel bar | Diameter: Ф4mm - Ф600mm |
| Nickel wire rod | Diameter:Ф0.01mm - Ф6mm |





Q1: Do you accept the trial order ?
A1: Yes,if we have the exactly size in stock.we can delivery even 1
piece/meter .
Q2: Can I have free sample before making orders?
|