| Brand Name: | FLYIN |
| Model Number: | Lithium Disilicate C14 |
| Certification: | CE |
| Place of Origin: | China |
| MOQ: | 1 pcs |
| Price: | USD 5-20 /pcs |
| Supply Ability: | 10000pcs/month |
| Delivery Time: | 5 work days |
| Translucency: | High |
| Material: | Lithium Disilicate |
| Sintering Temperature: | 900-950°C |
| Size Options: | 12mm, 14mm, 16mm, 18mm, 20mm |
| Manufacturer: | Dentsply Sirona |
| Coefficient Of Thermal Expansion: | 10.5 x 10^-6 K^-1 |
| Flexural Strength: | 400-500 MPa |
| Shade Options: | A1, A2, A3, A3.5, B1, B2, B3, C1, C2, C3, D2, D3, D4, Bleach |
| Indications: | Single crowns, inlays, onlays, veneers, anterior and posterior bridges |
| Chemical Solubility: | 0.2 μg/cm^2 |
| Radiopacity: | High |
| Color: | A1, A2, A3, A3.5, B1, B2, B3, C1, C2, C3, D2, D3, D4, Bleach |
| Vickers Hardness: | 500-600 HV |
| Company Info. |
| Shenzhen Flyin Technology co.,Ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
FLYIN The C14 Lithium Disilicate Block is a CAD CAM high esthetic denture material made of lithium disilicate
Product Description
| Model | Lithium Disilicate |
| Transparency | Low transparency 37%-41% High transparency 41%-44% |
| Density | 2.3-2.7g/cm2 |
| Chemical solubility | ≤100ug/cm2 |
| Vickers hardness | 5400±637MPa |
| Crystallization temperature | 840-850℃ |
1.High aesthetic restoration effect
2.High chemical stability and bending strength
3.Easy for milling, prolong use life of burs
4.Simple and fast crystallization process, less operation time
Dental Glass ceramic is a globally populardigital chairside
allceramic material, which is
easy to mill and crystallization process only takes 20 minutes,
with the CAD/cAM system of high
efficiency,precise production process precisely matched,advanced to
achieve instant restoration;
superior transparency,presenting a highly bionic aesthetic effect.
| Three-Point Bend Flexural Strength | 420±60 MPa |
| Density | 2.46-2.52 g/cm3 |
| Thermal Expansion Coefficient | 10.5*10 -6 /K (50-500°C) |
| Linear Shrinkage Rate | 0.10-0.26% |
| Vickers Hardness | 6500±200 MPa |
| Elastic Modulus | 50±10 GPa |
| Fracture Toughness | 2.8-3.8 MPa m-1/2 |
| Chemical Solubility | < 100 μg/cm2 |
|