| Sign In | Join Free | My benadorassociates.com |
|
| Categories | Nickel Alloy Plate |
|---|---|
| Brand Name: | Zhonggong Special Metallurgy |
| Model Number: | GH738 Alloy |
| Place of Origin: | China |
| MOQ: | 100KG |
| Price: | Price is negotiated based on the required specifications and quantity |
| Payment Terms: | Payment Terms: Mainly T/T.. L/C, D/A, D/P, |
| Supply Ability: | 5000 tons per month |
| Delivery Time: | 5-8 working days, depending on the parameters required for negotiation |
| Packaging Details: | Standard export packaging, or packaging as required |
| Density: | 8.19 g/cm³ |
| Melting Point: | 1260-1340°C |
| Tensile Strength: | 900-1100 MPa |
| Yield Strength: | 700-850 MPa |
| Elongation: | 20-35% |
| Hardness: | 250-300 HB |
| Thermal Conductivity: | 11.2 W/m·K |
| Oxidation Resistance: | Excellent |
| Applications: | Aerospace, Gas Turbines, High-temp. Components |
| Certification: | ISO Certificate |
GH738 Alloy is a high-performance, nickel-based superalloy engineered for exceptional mechanical strength and superior oxidation resistance at elevated temperatures. It is commonly used in aerospace and industrial gas turbine applications due to its ability to maintain structural integrity under extreme conditions.
Key Features:
GH738 Alloy’s robust performance characteristics make it a preferred choice for demanding applications where reliability and durability are paramount.
Here’s a table detailing the typical chemical composition of GH738 Alloy:
| Element | Content (%) |
|---|---|
| Nickel (Ni) | 50.0 - 60.0 |
| Chromium (Cr) | 20.0 - 25.0 |
| Cobalt (Co) | 7.0 - 10.0 |
| Molybdenum (Mo) | 3.0 - 5.0 |
| Titanium (Ti) | 2.5 - 4.0 |
| Aluminum (Al) | 1.5 - 2.5 |
| Iron (Fe) | Balance |
| Carbon (C) | ≤ 0.08 |
| Boron (B) | ≤ 0.01 |
| Other Elements | Traces |
This composition provides GH738 Alloy with its high-temperature strength and resistance to oxidation and corrosion.

|