| Brand Name: | Ruiyuan |
| Model Number: | PEEK |
| Certification: | UL/ISO9001/ISO14001/RoHS/Reach |
| Place of Origin: | China |
| MOQ: | 50kg |
| Price: | Negotiation |
| Payment Terms: | T/T |
| Supply Ability: | 100kg/week |
| Delivery Time: | 7 days |
| Packaging Details: | Carton |
| Contuctor Type: | Solid |
| Material: | Copper |
| Shape: | Rectangular |
| Width: | 2.0mm |
| Type: | Insulated |
| Certificates: | ROHS/UL/SGS/ISO9001:2008 |
| Product name: | High Temperature PEEK wire 2.0mm 4.0mm 5.0mm Enameled Flat Copper Wire |
| Thickness: | 1.4mm |
| Company Info. |
| Tianjin Ruiyuan Electric Material Co,.Ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
PEEK wire is used in a variety of applications due to its exceptional properties. Here are some common uses:
Aerospace: PEEK wire is used in aircraft components and systems that require lightweight materials with high strength and thermal stability.
Medical Devices: In the medical field, PEEK wire is utilized for surgical instruments, implants, and other devices that must withstand sterilization processes and maintain biocompatibility.
Electronics: PEEK wire serves as insulation for electrical wiring in high-temperature environments, such as in motors, sensors, and connectors.
Automotive: It is used in automotive applications for components that need to endure high temperatures and harsh chemicals, such as in fuel systems and electrical systems.
Oil and Gas: PEEK wire is employed in downhole applications where resistance to extreme temperatures and corrosive environments is essential.
Industrial Applications: It is used in various industrial settings for components that require durability and resistance to wear and chemicals.
Overall, PEEK wire is valued for its ability to perform reliably in demanding conditions, making it suitable for high-performance applications across multiple industries.
Ref. - | Item | Specification | Measurement data | Measure equipment | |
| No. | W607010 2A250904 | W607010 2B250904 | |||
| 1 | Copper width | 1.980-2.020mm | 2.004 | 2.005 | Mircometer |
| 2 | Copper thickness | 1.380-1.420mm | 1.400 | 1.399 | Mircometer |
| 3 | Overall width | 2.300-2.360 mm | 2.324 | 2.321 | Mircometer |
| 4 | Overall thickness | 1.700-1.760 mm | 1.732 | 1.731 | Mircometer |
| 5 | Copper radius | 0.350-0.450mm | 0.375 | 0.408 | Microscope |
| 6 | Copper radius | 0.385 | 0.412 | Microscope | |
| 7 | Copper radius | 0.399 | 0.411 | Microscope | |
| 8 | Copper radius | 0.404 | 0.407 | Microscope | |
| 9 | Insulation layer thickness | 0.145-0.185mm | 0.170 | 0.159 | Microscope |
| 10 | Insulation layer thickness | 0.162 | 0.155 | Microscope | |
| 11 | Insulation layer thickness | 0.155 | 0.161 | Microscope | |
| 12 | Insulation layer thickness | 0.167 | 0.165 | Microscope | |
| 13 | Insulation layer thickness | 0.152 | 0.155 | Microscope | |
| 14 | Insulation layer thickness | 0.161 | 0.159 | Microscope | |
| 15 | Insulation layer thickness of radius | 0.145-0.185mm | 0.156 | 0.158 | Microscope |
| 16 | Insulation layer thickness of radius | 0.159 | 0.155 | Microscope | |
| 17 | Insulation layer thickness of radius | 0.154 | 0.159 | Microscope | |
| 18 | Insulation layer thickness of radius | 0.160 | 0.165 | Microscope | |
| 19 | Copper | T1 | OK | Material certificate | |
20 | Coating/Temperature grade | 240℃ | OK | Material certificate | |
| 21 | Elongation | ≥40% | 46 | 48 | Tensile tester |
| 22 | Spring back angle | / | 5.186 | 5.098 | Auto spring back test |
23 | Flexibility | After winding with Ø 2.0mm and Ø3.0mm diameter round rods, there should be no cracking in the insulation layer. | OK | OK | Visual |
| 24 | Adhesion | ≤3.00mm | 0.394 | 0.671 | Tensile tester&Microscope |
| 25 | 20℃ Conductor resistance | ≤6.673 Ω/km | 6.350 | 6.360 | Conductor resistance tester |
| 26 | BDV | ≥12000 V | 22010 | 21170 | Auto voltage tester |
27 | PDIV | ≥1300 RMS (25℃,50V/S,50Hz,100Pc) | 1425 | 1429 | PDIV tester |
28 | Heat shock | After baking at 240℃ for 30 minutes, the insulation layer should have no cracks. | OK | Oven | |
29 | Defect inspection | High voltage Pinhole: DC 3000V, 16uA | 0 | 0 | On-line inspection system |
| Parricle: Height>0.100mm need to be marked | 0 | 0 | |||
Impurity:Length or width ≥ 0.4mm or area ≥0.16mm² need to be marked | 0 | 2 | |||
30 | Spool&Weight | Sample phase:P-30,25±15kg Mass productin:PC-630B,160± 60kg | P-30 | P-30 | Visual |

|